Abstract
The polymeric compounds of epoxy as the base material were studied and prepared with sulfur in different weight percentages (1%, 3%, 5%, 7%, 9%, 11%) as reinforcement materials and at different temperatures, It was found that after obtaining the results and comparing before and after the reinforcement of the prepared models, the thermal conductivity values decreased, but the hardness values increased at 52 °C and decreased at 22 °C, in contrast to the measurements of the resistance (impact, compression) increased at 22 °C and decreased at 52 °C
Keywords
(Compression
epoxy
Impact).
Sulfur
thermal conductivity